carrier of the print, i. e. the paper or card»
board is discolored under the influence of
the sun rather quickly and by its yellowish
tan it alters the shades of the inks trans-
parently printed thereon. Therefore for the
highest claims only paper stock is to be
selected that in itself answer these re-
quirements.
Last but not least is to be considered the
consistency and the degree of concentrat-
ion of the ink to be used for printing, also
whether it is a surface printing or a three:
quarter, half or quartertone. The amount
of coloring bodies placed on a square
centimeter is of utmost importance for the
resistance to light. T'he full surface printed
with the unreduced ink is always more
resistent than the threequarter, half or
quartertone which on top of it all may
even be applied by means of a reduced
solution of the ink. By the same reasons
may be stated that the full colour ink is
always faster to light than any reduced
substance produced from the full colour
ink. Very important is the often misjudged
fact that a printing ink of first class fastness
to light mixed with another ink of second
class does not necessarily produce an ink
the fastness of which ranges from ı to 2,
its fastness to light in the majority of cases
remains rather below the class to which
belongs the less fast printing ink. Finally,
whilst discussing the order with the custo+
mer he should be asked to explain where
the respective printing matter which he
insists to be fast to light is supposed to be
placed or exhibited. It should be pointed
out to him that for instance a shows
package placed in a shopswindow to the
North requires much less power of re
sistance than if it were to be exhibited in
a show»window placed to the South and ex-
posed to the sun during the whole day. His
attention is to be drawn to the fact that
the influences of temperature and air too
bear considerable influence on the fastness
to light; in high temperature the paper
discolors by turning to a yellowish tint
much quicker than it will in low tem-
perature and the ink too will display less
resistance. Humidity of the air above the
normal and fumes in the neighborhood of
factories and railway lines and yards too
are to be considered as influential factors
with the discoloring of printing matters.
A customer placing an order with some
Printing plant will certainly not lay claims
on an absolute fastness to light if he has
been duly notified of these particularities,
but he will be contented if the most
resistent paper and the fastest ink has been
chosen and properly used for his order.
No printing establishment can promise
more than that.
B. Kesistence to alkali
Wrappings for instance for soap or wash-
powder must be resistent to alkali and
therefore they are to be printed with print:
ing inks resistent to alkali. How is the
claim of resistance to alkali established and
how is the printing ink’s resistance to alkali
proved? The “Commission for the Nor;
malization within the Graphic Trade” pro:
claims the following definition: Resistance
to alkali is the resistance of the print
against alkaline reacting substances. It is of
importance for instance when the paste
contains alkaline substances, especially also
in wrappers for wash-powder, soda and
similar materials.
The control whether the ready print is
resistent to alkali is performed in the
following way: over a stripe of the ready
print measuring about 10x 2,5 geal:
meters about 47x 1%). in a testsglass is
poured at normal temperature a 1% solut;
ion of natron Iye, after the lapse of 5 minus
tes it is removed from the test-glass, rinsed
with distilled water and dried at 5o degree
Celsius. A print resistent to alkali should
not display any noticeable alterations. r
Typically resistent colour: Ultramarin .
Typically not resistent colour: “Berlin
Blue”.
A printing establishment having used
printing inks resistent to alkali for a job
requiring this resistance and to which the
above test has been successfully applied,
technically has performed the job accords
ing to rule. Practically, however, it is nearly
always of advantage for all parties con-
cerned when the printer inquires further
into the particulars which establish the
demand for resistance to alkali in the print:
ing job required by his customer, because
thereby certain shortcomings may be
eliminated from the very start and many
subsequent claims are avoided.
A discoloring of the print by alkali prin-
cipally is possible only if the humidity of
the material wrapped is unusualy high or
ifthe humidity is absorbed during storage,
so that the very alkaline reaction is pro:
duced. The humidity absorbs the respec»
tive alkaline substances and produces the
reaction on the paper and in the ink as
performed by a more or less concentrated
solution. This, of course, occurs when the
humidity of the contents penetrates the
protective wrapping and reaches the print»
ed cardboard, passing finally this too from
within to reach the outer side of the card-
board the surface of which carries the
print. In this process at first the paper or
the cardboard respectively is attacked, the
Fibre of the paper swells and turns yellow,
the sizing of the paper is destructed, the
glazing suffers and the surface looses its
smoothness. It is understood that with such
fundamental alterations in the paper’s con+
ditions also the printing is to suffer, even
when printing ink of a quality resistent to
alkali has been adopted! Thus for instance
a blue ink resistent to alkali will turn to a
greenish tint on yellowish paper. Paper,
however, that may claim absolute re
sistance to alkali does not exist and thus
the supreme rule is that in the first place
the goods are to be packed in perfectly
dry conditions (especially also soap!) and in
the second place the filled packs are to be
stored perfectly dry, for dry alkaline sub»
Seinees attack neither paper nor printing
ink. — Here too, of course, it is of ims
portance that no unresistent materials or
substances are to be added to or mixed
with the originally resistent paper material
and that Printing inks unfit with regard to
resistence to alkali are not mixed with
printing inks resistent to alkali. Further;
more it should be ascertained before pers
forming the print, whether the substances
to be wrapped up in the pack do not
contain either grease, solution substances,
ethereal oils, &c. which bear an influence
on the colour and on the printing. After
having considered and solved all these
questions the present standard of science
and technique will warrant at any rate that
by due cooperation between the Printer, the
paper;miller and the printing-ink manus
facturer a wrapper can be produced that
answers sufficiently to all requirements,
There is to be reckoned with a certain
alteration in the shades for which due
allowance should be reserved beforehand
so that differences of colour between the
projected print and the final ready print
may be accounted for, yet the allowance
made for such slight variations never works
out as detrimental, as that the showpack on
&hibition in the shop-window may prove
unfit to answer the claims laid on it by
turning into a cheap-looking object.
C. fastnesg to greage
Similarly as many oily substances the
commercially handled alimentary grease
substances dissolve a number of dry inks.
Thus printing inks containing coloring
substances solvable in oil or grease are not
suitable for the Printing of wrappers for
butter, margarine or other greasy materials
and fat, because the eoloring substances by
141