Text on this page (OCR)

ETCHING
the lines drawn with the ‘needle’ may show clearly, the ground is blackened, or
‘smoked,’ by holding the plate face down, by a hand vise attached to one corner,
and passing a lighted wax taper back and forth over it. The drawing is made with
a sharp pointed steel needle, the function of which is not to make the line in the
plate but, by penetrating the thin ground, to expose the copper for the acid to
attack later.


“When the drawing is completed the plate is immersed in dilute acid, preferably
nitric or hydrochloric; or the mordant may be applied with a feather or brush. As
soon as the lightest lines have been ‘bitten,’ the artist removes the plate from the
acid and covers up these lines with varnish to protect them from further etching,
The process of biting and ‘stopping out’ is then repeated until the required depth
is obtained for the lines which are to count darkest in the print.”


GROUNDING
Eighteen-gauge copper always. It is stiff enough and not so thick that the edges of
the plate, when a little beveled, punch through the paper in printing.


The first problem and one of the most important is to see that the plate is clean
(and I mean clean). No ground will stand up under the ordeal of biting if it is put on
an even remotely greasy plate, and there is nothing more heartbreaking than a
ground that cracks up under the acid. There is nothing to do about it. I make sure
of this first and greatly important ground by going over the whole plate in several
directions with a large piece of charcoal and water. This not only removes all
grease but the machine polish of the plate as well, and leaves the surface mellow
and amenable to future working.


It is obvious that the later cleaning and grounding, for either re-biting or addi-
tional work, must be different. The plate must be made clean some other way.
There are several liquids used for this—acetic acid, vinegar and salt, chloroform,
and others. I have used them all but from some inherent personal grubbiness per-
haps or maybe because of the metal polish I like, none of them seem to work for me.
There was endless trouble. But just lately, taking a tip from an advertisement, I
have been using a thin solution of just common lye, rinsed off well after application.
It seems to be sure fire and I do not think harms the plate—but look out for fingers!
My test for a clean plate is when water will flow all over it and not run together
in spots.


There are three ways of grounding the plate. First, floating it on in liquid form
and then setting the plate on edge to drain. Second, warming the plate sufficiently
to melt the solid ground which is then distributed evenly over the surface with a
dabber; and third, the same as the second except that the distribution is done with


42

Open this record in the IADDB collection viewer