Commercial Art / Art and Industry, November 1933 – page 33

Commercial Art / Art and Industry, November 1933 – page 33
Magazine
Commercial Art / Art and Industry
Issue date
November 1933
Page
33
Department
Magazines and journals
Object number
CAI_1933-11-01_p33

Text on this page (OCR)

removed. ‘This is achieved by a process known as ~ routing.” Routing is done by a


machine operating a high-speed cutting spindle. The spindle is guided by the operator's
hand control of a radial arm.


The work of hands, feet and eyes must be controlled together


Cutting depth is controlled by one foot. and the other foot
controls the power unit.
with the utmost precision. After inspection and proofing, the plate is ready for mounting
and dispatching.


Line blocks are occasionally engraved on copper if the subject contains any exceptionally
intricate drawing, as in such cases a better result is obtained due to the finer grain of the
metal and the different method of etching. Line engravings on copper cost twice as much
as those on zinc.


The line reproduction can be elaborated by the judicious application of mechanical tints,
Any process-engraver can supply printed sheets showing specimens of the different tints
he stocks. The tints are identified by numbers.


The effect of the use of mechanical tints on an open line drawing is illustrated.


The process by which these mechanical tints are worked into a reproduction of a line
drawing is known as tint-laying. The drawing is photographed to the desired size on to a
sensitised glass plate, forming the negative, as already described. Thenegative is developed,
intensified and printed on to zinc in the usual manner. Then gum is painted over every
part of the image where the tint is not required.


The mechanical tints themselves are sheets of either hardened gelatine or celluloid, with
smooth backs and relief printing surfaces. The printing surfaces are made in a variety of
patterns. These relief sheets are mounted in wooden frames with metal corners.


When these relief printing surfaces receive a spread of ink, the patterns or tints can be
transferred to the metal carrying the image. The operator applies an even surface of
transfer ink to a hand roller and rolls the surface of the tint, which is then laid over the
zine sheet carrying the image. Pressure being applied, the tint is printed over the surface
of the metal. The parts over which the tint is required are coated with bitumen powder
to form an acid resist.


The plate is now washed in water, which removes all of the superfluous surface of the
tint, leaving it only where actually w anted. This is due to the fact that the gum previously
applied is soluble in water, whereas the combination of the ink with bitumen powder is
insoluble. Gum causes desensitisation of the plate ; accordingly, it is next given a bath in
a very weak nitric acid solution and then dried over a burner. The plate then proceeds
to the etching room, where it is etched as previously described.


It will be readily perceived that, by this system, any number of tints can be applied
to different parts of the image.


You will notice in the illustration showing a selection of tints that, under each tint,
in addition to the identification number, a set of dimensions is given. These figures refer
to the area of the sheet carrying the printed pattern, and show, therefore, the extreme
measurements available for the laying of the tint in question. The sizes, of course, apply
to the reduced size of the reproduction— -not to the correspondingly larger area on the
original sketch.


The correct method of specifying mechanical tints when ordering is to place a sheet of
tracing paper over the drawing, pasting it down at the top, and to shade, in blue pencil,
the section of the illustration where the tint is required, also indicating the number of the tint.


Choice of tints may often be left to the discretion of the photo-engraver. In fact, this

Open this record in the IADDB collection viewer